Tensile Strength (Mpa or N/mm²) |
500 - 600 |
1000+ |
Shear Strength (Mpa or N/mm²) |
120-150 |
170 - 200 |
Bond Strength (Mpa or N/mm²) |
14* |
08 - 23 |
Compression (Mpa or N/mm²) |
500 |
450 > |
Concrete Covering |
Standar Covering |
Can be reduced upto 40% |
Modulus of Elasticity (Gpa) |
160 - 200 |
45 - 65 |
Elongation (%) |
25 |
1.5 - 2.5 |
Durability |
20 Years |
80 Years+ |
Density (Ton/m³) |
7.8 |
1.9 |
Corrosion Resistance to Aggressive Environment |
Highly Corrosive |
Non Corrosive |
CO2 Emission |
High Emission |
Low Emission |
Electrical Conductivity |
Electrically Conductive |
Non Conductive |
Cyclic Load |
20,000 Cycles |
4,20,000 Cycles |